Dustless blasting vs. Soda blasting

Bdhand

Contributor
Sr. Member
Joined
Aug 15, 2015
Messages
712
Hey guys what's your take on the Dustless blasting that uses water and glass vs. soda blasting for the frame and body. I am looking at doing either one and was wondering if anybody had any luck with either or. I have a guy local that will do my frame and body for 600.00 with the dustless blasting. I have heard that if you soda blast and you don't get all of the soda off of the vehicle that it could cause you problems down the road with wiring and paint. Let me know what you guys think

Thanks,
Brent
 

DirtDonk

Contributor
Bronco Guru
Joined
Nov 3, 2003
Messages
51,651
Around here that's a pretty decent price for any kind of blasting.
If coming to your location, dustless would be preferred just for the mess. But I do believe (and others can confirm or refute) that the liquid in the dustless method should keep the parts cooler as well. Which can be a HUGE benefit to the thinner sheet metal stuff.

The frame and suspension couldn't care less about heat buildup, but some body panels (hoods, grilles, etc) can't handle the heat.
Of course, no matter what method they need to take extra caution on the hard tops, the hoods and the grilles just to keep from warping any metal not just from heat, but from the force of the blast.
I'm guessing they know their business, but you do have to mention that stuff anyway in case they're newer at it.

Paul
 

AZ73

Bronco Guru
Joined
Mar 28, 2012
Messages
3,813
If you do soda you'll have to either use an etching primer or scuff it makes the metal comes out smooth. In theory, the rust inhibitor in "dustless" allows any primer up to 72 hours after the blast. I've also heard that soda gets everywhere and you have to really blow it out before you paint or the pressure from the spray gun will scatter it all over your new paint. I use glass in a cabinet and it leaves a nice, "rough" finish. In fact I use it to "matte" polished aluminum
 

RPM289

Sr. Member
Joined
Jan 4, 2008
Messages
835
I have the access to a dustless blaster system my brother stripped a 69 cougar in about an hour. I did frame axles and most of the body parts on the 52 jeep project great system does great.
 

RPM289

Sr. Member
Joined
Jan 4, 2008
Messages
835
Around here that's a pretty decent price for any kind of blasting.
If coming to your location, dustless would be preferred just for the mess. But I do believe (and others can confirm or refute) that the liquid in the dustless method should keep the parts cooler as well. Which can be a HUGE benefit to the thinner sheet metal stuff.

The frame and suspension couldn't care less about heat buildup, but some body panels (hoods, grilles, etc) can't handle the heat.
Of course, no matter what method they need to take extra caution on the hard tops, the hoods and the grilles just to keep from warping any metal not just from heat, but from the force of the blast.
I'm guessing they know their business, but you do have to mention that stuff anyway in case they're newer at it.

Paul

Good advise :) I have played with ours on a scrap horizontal stab from a airplane its .024 aluminum I hit it pretty hard with medium media and it made surface rough but did not warp it up any so the water keeps it cool but at 100psi you have to be careful.

Let me know if anyone in NC area needs blasting done ;D;D
 

Case

Sr. Member
Joined
Dec 7, 2003
Messages
855
If you do soda you'll have to either use an etching primer or scuff it makes the metal comes out smooth. In theory, the rust inhibitor in "dustless" allows any primer up to 72 hours after the blast. I've also heard that soda gets everywhere and you have to really blow it out before you paint or the pressure from the spray gun will scatter it all over your new paint. I use glass in a cabinet and it leaves a nice, "rough" finish. In fact I use it to "matte" polished aluminum
thanks for posting this, I am about to start soda blasting my 72 and didnt know i would need to either use a self etching primer or scuff up the metal.
 
Top